AWS A5.13 ECoCr-A paʻakikī ke alo o ka manual electrode weld fabrication jointing

ʻO GEH-SL6 He electrode i hoʻokumu ʻia i ka cobalt e like me ka maʻamau AWS A5.13 ECOCRA-A.Hoʻohana nui ʻia no ka hoʻoulu ʻana i ka wela kiʻekiʻe a me ke kiʻekiʻe kiʻekiʻe kiʻekiʻe kiʻekiʻe kiʻekiʻe, nā ʻili wela wela, nā ʻenekini pahu, turbine blades, etc. Hiki ke hoʻohana ʻia no ka AC a me DC.Pono e hoʻohana i ka pilina hoʻohuli DC a me ka pilina pili electrode.Paʻa paʻa, uhi slag maikaʻi, ʻano nani.Loaʻa i ka papa i luna nā waiwai mechanical piha piha i ka pae wela kiʻekiʻe ma lalo o 800 ℃, a he kūpaʻa maikaʻi i ka corrosion, pale ʻana a me ke kūpaʻa ʻana i ka lole intermetallic.Hiki ke hoʻohana ʻia ka papa i luna.


  • Brand::Gintune
  • 'ikamu helu::GEH-SL6
  • Pono no::Paʻa paʻa o ka valve
  • Polarity lako mana::DC+
  • Mana palapala::AOLE
  • Kūlana welding: ʻO AWS A5.13 ECoCr-B ka hoʻohui ʻana i ka uea wili wili i ke alo paʻakikī.
  • Huahana Huahana

    Seocification

    Huahana Huahana

    Hoʻohana & Kūlana

    ʻO GEH-SL6 kahi ʻano hoʻoheheʻe i luna no ka valve engine, turbine blade, kiʻekiʻe kiʻekiʻe a me ke kiʻekiʻe kiʻekiʻe kiʻekiʻe kiʻekiʻe, wela forging die a me nā ʻāpana pale ʻana o ka wela wela a me nā ʻāpana kūʻē i ka corrosion.I ke kaʻina hana kuʻi, i mea e paʻa paʻa me ka substrate, pono ia e weld i ke komo hohonu.No laila, hiki ke hoʻohana ʻia ke ʻano kuʻihao pōkole pōkole wale nō.ʻO ka lua, i mea e hoʻoponopono ai i ka pilikia o ka wai hohonu a me ka hoʻoheheʻe ʻana o nā mea kumu nui i ka weld i ka wā pōkole arc welding, kiʻekiʻe ka dilution rate.ʻO ka nele o nā mea hana i loko o ka weld layer e hōʻemi i ka pilikia pale pale.Pono e hoʻohana i ke ʻano o ka hoʻopili ʻana i ka ʻili he nui.Ma kēia ʻano, ʻaʻole wale nā ​​ʻāpana kūpono a me ke kūpaʻa ʻana i ka ʻaoʻao hope e hoʻonui i ka papa ma ka papa.Eia kekahi, ʻo nā papa mua o ka ihu e pāʻani i ke ʻano o kahi papa hoʻololi, e hōʻemi ana i ka māwae ma muli o ka ʻokoʻa o ka hoʻonui ʻana o ka wela ma waena o nā papa ʻelua e pili ana.I kēia manawa, pono e hoʻohana ʻia ke ʻano o ka neʻe ʻana o ka laina pololei, ke ʻano o ka neʻe ʻana o ka iʻa, ke ʻano o ka herringbone a i ʻole ka pōkole arc agitation neʻe.

    Nā hiʻohiʻona

    ʻO kēia ka titanium calcium coating cobalt base surfacing electrode, kūpono no ka DC reverse connection, hiki i ka metala i luna ke hoʻomau i ke kūpaʻa maikaʻi a me ka pale ʻana i ka corrosion ma 650 ℃, ka hopena a me ke anuanu a me ka wela wela.Hiki ke hoʻohana ʻia i nā koi a puni 650 ℃ hana hiki ke mālama i ke kūpaʻa ʻaʻahu maikaʻi a me ke kūpaʻa corrosion, a me ka hopena a me ke anuanu a me ka wela staggered wahi, hiki ke hana maikaʻi.

    Nā kila Carbon kiʻekiʻe
    未标题-2

    Hui & Hale Hana

    hale hana2

    ʻO ka hoʻohui ʻana o ka huahana a me ka hoʻokomo ʻana i nā waiwai mechanical

    KOMPONO KIMIKA:

    ALLOY(wt%) C Mn Si Cr Ni Mo Fe W Co
    GB/T RULA 0.70-1.40 2.00 2.00 25.00-32.00 - - 5.000 36.00 hoomaha
    NA RULA AWS 0.7-1.4 2.00 2.00 25-32 3.00 1.00 5.00 3.0-6.0 hoomaha
    KA WAIWAI LA'ANA 1.03 1.28 1.11 30.1 2.4 0.1 3.65 4.420 hoomaha

    PALAPALA PALAPALA I MANAOIA:

    NĀ KĀNĀWAI (mm) 3.2*350 4.0*350 5.0*350
    UILA
    (Amp)
    120-160 140-190 150-210
    asgvsbsb

    NA HIHIA MAU

    430Mpa Electrode lima no ka hao kalapona haahaa05
    典型项目

    Palapala

    palapala hōʻoia

    ʻO ka hoʻohui ʻana o ka huahana a me ka hoʻokomo ʻana i nā waiwai mechanical

    KOMPONO KIMIKA:

    ALLOY(wt%) C Mn Si Cr Ni Mo Fe W Co
    GB/T RULA 0.70-1.40 2.00 2.00 25.00-32.00 - - 5.000 36.00 hoomaha
    NA RULA AWS 0.7-1.4 2.00 2.00 25-32 3.00 1.00 5.00 3.0-6.0 hoomaha
    KA WAIWAI LA'ANA 1.03 1.28 1.11 30.1 2.4 0.1 3.65 4.420 hoomaha

    PALAPALA PALAPALA I MANAOIA:

    NĀ KĀNĀWAI (mm) 3.2*350 4.0*350 5.0*350
    UILA
    (Amp)
    120-160 140-190 150-210

     

     