ʻO ke kila kila kila Electrode E309L-15 ke kila kila a me ke kila kuhili ʻole
IKE NUI WELDING
Mai ʻae i nā nīnau
E hoʻomau mau iā ʻoe
Paʻa ʻole ʻo Arc
ʻO ka hoʻoheheʻe ʻana
ʻO ka pipiʻi nui
Hoʻohana pinepine ʻia no ke kila like ʻole
wiliwili o ke kila kila a me ke kila kalapona.
A i ʻole i hoʻohana ʻia i ka ʻino ʻino o ka martensite, ferritic stainless steel welding.
Maikaʻi ka ripple
Haʻahaʻa hydrogen kuhiliʻole lima electrode, ka mea nui he haʻahaʻa C-22% Cr-12% Ni, haʻahaʻa kalapona maʻiʻo a me ka maikaʻi māwae kū'ē.
ʻO ka hana kuʻi ʻana maikaʻi, kūpaʻa arc, hana nani,
nane liʻiliʻi, paʻipaʻi liʻiliʻi, wehe ʻia ka palapa maʻalahi;
Loaʻa ka pale ahi maikaʻi, kūpaʻa porosity maikaʻi,
paʻa mechanical waiwai o ka metala hehee, a kiʻekiʻe X-Ray pass rate.
ʻO ka slagging maʻalahi
Laina Huahana
KOMPONO KIMIKA:
ALLOY(wt%) | C | Mn | Si | P | S | Ni | Cr | Mo | Cu | 'ē aʻe |
GB/T RULA | 0.032 | 1.06 | 0.67 | 0.027 | 0.006 | 13.25 | 23.6 | 0.04 | 0.01 | - |
WAIWAI MECHANICAL:
WAIWAI | IKAIKA HUA(MPa) | KA IKAIKA HOU (MPa) | KA WAIWAI IMAPACT J/℃ | Hana wela °C*h | ||||
GB/T RULA | 595 | 38 | - | - |
PALAPALA PALAPALA I MANAOIA:
NĀ KĀNĀWAI (mm) | 2.0*250 | 2.6*300 | 3.2*350 | 4.0*350 | 5.0*350 | |||||
UILA (Amp) | H/W | 30-55 | 50-85 | 80-120 | 100-150 | 140-180 | ||||
O/W | 20-50 | 45-80 | 70-110 | 90-135 | - |
Kākoʻo hale hana
He kūpono ka huahana no kahi
laulā o nā noi
IKE NUI WELDING
-
ʻO nā mea wili no nā alumini alumini
-
ʻEkolu puka 2# ʻaʻole hana
-
300,000-ton ka lawe nui
KOMPONO KIMIKA:
ALLOY(wt%) | C | Mn | Si | P | S | Ni | Cr | Mo | Cu | 'ē aʻe |
GB/T RULA | 0.032 | 1.06 | 0.67 | 0.027 | 0.006 | 13.25 | 23.6 | 0.04 | 0.01 | - |
WAIWAI MECHANICAL:
WAIWAI | IKAIKA HUA(MPa) | KA IKAIKA HOU (MPa) | KA WAIWAI IMAPACT J/℃ | Hana wela °C*h | ||||
GB/T RULA | 595 | 38 | - | - |
PALAPALA PALAPALA I MANAOIA:
NĀ KĀNĀWAI (mm) | 2.0*250 | 2.6*300 | 3.2*350 | 4.0*350 | 5.0*350 | |||||
UILA (Amp) | H/W | 30-55 | 50-85 | 80-120 | 100-150 | 140-180 | ||||
O/W | 20-50 | 45-80 | 70-110 | 90-135 | - |